Espesor: 0.3mm-1.2mm

     
    Recubrimiento de zinc: 40g / m2-150g / m2


    Espesor de la pintura: 25mic / 5-10mic

     


    Thickness: 0.3mm-1.2mm

     

    Zinc Coating: 40g/m2-150g/m2

     

    Painting Thickness: 25mic/5-10mic

Detalle del Producto

Especificación del Acero PCM:
1) Grueso: 0.3mm-1.2mm
2) Revestimiento de zinc: 40g / m2-150g / m2
3) Grosor de la pintura: 25mic / 5-10mic
4) Anchura estándar: 914mm, 1000m m, 1200m m, 1270m m o por la petición.
5) Peso de la bobina: por solicitud.
6) DI: 508mm / 610mm
7) Color: RAL u otras series
8) El revestimiento sostiene una flexión de 180 grados


Procesamiento del Acero PCM:

Pay-off de bobina → corte de doble corte → soldador-anotador → acumulador de entrada → pre sección de limpieza → horno → brida caliente → pote de zinc → cuchilla de aire → enfriador → lavado por agua → secador → laminación de acabado → secador → nivelador de tensión → secador → Revestimiento químico → Horno químico → Enfriador → Acumulador de salida → Lubricante → Curva de salida → Carrete de tensión.


El equipo seleccionado es indispensable para la calidad superior. El equipo de laminador en frío de metal de Shanghai fue importado de SMS Demag de Alemania y de Italia.
Tan raras eran las compañías nacionales que poseían instalaciones de procesamiento avanzadas tan mundanas. Las líneas de decapado, regeneración ácida y galvanización por inmersión en caliente que se corresponden con el molino en frío también se compran en empresas nacionales bien conocidas. Estos avanzados equipos de producción seguramente han sentado una base sólida para la producción de productos superiores.




Specification of PCM Steel:
1) Thickness: 0.3mm-1.2mm
2) Zinc Coating: 40g/m2-150g/m2
3) Painting Thickness: 25mic/5-10mic
4) Standard Width: 914mm, 1000mm, 1200mm, 1270mm or by request.
5) Coil weight: by request.
6) ID: 508mm/610mm
7) Color: RAL, or other series
8) Coating sustains 180 degree bending
 
Manfacturing Process of PCM Steel:
Pay off reel → double cut shear → welder-notcher → entry accumulator → pre cleaning section → furnace → hot bridle →

zinc pot → air knife → after cooler → water quench → dryer → skin pass mill → dryer → tension leveler → dryer →

chemical coater → chemical oven → cooler → exit accumulator → oiler → exit shear → tension reel. 



Selected equipment is indispensable for superior quality. Shanghai metal cold rolling mill equipment was imported from SMS Demag of Germany and from Italy.

So rare were any domestic companies to own so worldly advanced processing facilities. The pickling, acid regeneration, and hot-dip galvanizing lines matching

the cold mill are also purchased from well-known domestic companies. These advanced production equipments have surely laid a solid foundation for producing

superior products.
 

Aplicaciones del Acero PCM:
Se utiliza para los aparatos eléctricos, tales como refrigerador; lavadora; microonda; DVD, etc.

 

Application of PCM Steel:

it is used for electric appliances, such as refrigerator; washing machine; microwave; DVD;etc. 

SOLICITE UNA COTIZACIÓN AQUÍ
SOLICITE
UNA
COTIZACIÓN
AQUÍ

NOSCOMUNICAREMOS CON USTED DENTRO DE LAS 8 HORAS

* E-mail:Double check your email address, maybe you have spelling mistakes, thanks.
* Nombre de Companía:
País:
* Detalle:
 cargar: visitor